Sino's inclusion stains solve the problem that cadmium red can't resist high temperature.

They are very stable in the glaze which contains lead, calcium, or boron. If the content of the alkali metal in the giaze is too high, it will damage the included layer of the stains, and alsodegrade the color. So the grinding of the stain can't last long time.

The temperature range covers:800-1280℃

 
Code No Name Composition Max Firing Temp Firing condition Color
SIS300B Pale Yellow Cd-Si-Zr-S 1280 Oxidation  
SIS300 Golden Yellow Cd-Si-Zr-S 1280 Oxidation  
SIS300A Dark Yellow Zr-Si-V 1280 Oxidation  
SIS301C Orange Yellow Al-Co-Zn 1280 Oxidation  
SIS301 Orange Yellow Cd-Si-Zr-Se-S 1280 Oxidation  
SIS301A  Orange Yellow Cd-Si-Zr-Se-S 1280 Oxidation  
SIS301B Orange Red Cd-Si-Zr-Se-S 1280 Oxidation  
SIS306 Red Cd-Si-Zr-Se-S 1280 Oxidation  
SIS306A Red Cd-Si-Zr-Se-S 1280 Oxidation  
SIS306B Red Cd-Si-Zr-Se-S 1280 Oxidation  
SIS306C Dark Red Cd-Si-Zr-Se-S 1280 Oxidation  
SIS309  Dark Red Cd-Si-Zr-Se-S 1280 Oxidation  

Note:The color marks shown are only for reference as they may vary from those of the actual products.